Uns N06600 Sheet Thickness Chart

Måler (ga) Ståltykkelse (in.) Ståltykkelse (mm) Aluminiumstykkelse (in.) Aluminiumstykkelse (mm)
3 0.2391 6.07 0.2294 5.83
4 0.2242 5.69 0.2043 5.19
5 0.2092 5.31 0.1819 4.62
6 0.1943 4.94 0.162 4.11
7 0.1793 4.55 0.1443 3.67
8 0.1644 4.18 0.1285 3.26
9 0.1495 3.80 0.1144 2.91
10 0.1345 3.42 0.1019 2.59
11 0.1196 3.04 0.0907 2.30
12 0.1046 2.66 0.0808 2.05
13 0.0897 2.28 0.072 1.83
14 0.0747 1.90 0.0641 1.63
15 0.0673 1.71 0.0571 1.45
16 0.0598 1.52 0.0508 1.29
17 0.0538 1.37 0.0453 1.15
18 0.0478 1.21 0.0403 1.02
19 0.0418 1.06 0.0359 0.91
20 0.0359 0.91 0.032 0.81
21 0.0329 0.84 0.0285 0.72
22 0.0299 0.76 0.0253 0.64
23 0.0269 0.68 0.0226 0.57
24 0.0239 0.61 0.0201 0.51
25 0.0209 0.53 0.0179 0.45
26 0.0179 0.45 0.0159 0.40
27 0.0164 0.42 0.0142 0.36
28 0.0149 0.38 0.0126 0.32
29 0.0135 0.34 0.0113 0.29
30 0.012 0.30 0.01 0.25
31 0.0105 0.27 0.0089 0.23
32 0.0097 0.25 0.008 0.20
33 0.009 0.23 0.0071 0.18
34 0.0082 0.21 0.0063 0.16
35 0.0075 0.19 0.0056 0.14
36 0.0067 0.17 – –

 

600 Alloy Plate Tykkelse Chart

Måler LB/Sq. Ft. LB/Sq In. Platemålertoleranse
72 tommer bred 96 tommer bred
3/16 0.1875 8.579 0.05958 +.045″ -.010″ +.050″ -.010″
7/32 0.2187 9.870 0.06854
1/4 0.2500 11.162 0.07750
5/16 0.3125 13.746 0.09546
3/8 0.3750 16.496 0.11456 +.055″ -.010″ +.060″ -.010″
7/16 0.4375 19.080 0.13250
1/2 0.5000 21.633 0.15044
9/16 0.5625 24.247 0.16838
5/8 0.6250 26.831 0.18633
11/16 0.6875 29.415 0.20427
3/4 0.7500 32.123 0.22308 +.060″ -.010″ +.065″ -.010″
13/16 0.8125 34.707 0.24102
7/8 0.8750 37.291 0.25897
15/16 0.9375 39.875 0.27691
1 1.0000 42.665 0.29628 +.070″ -.010″ +.075 -.010″
1-1/8 1.1250 47.833 0.33217
1-1/4 1.2500 53.001 0.36806
1-3/8 1.3750 58.169 0.40395
1-1/2 1.5000 63.337 0.43984
1-3/4 1.7500 73.672 0.51161
2 2.0000 84.008 0.58339 +.125″ -.010″ +.150″ -.010″
2-1/8 2.1250 89.610 0.62229
2-1/4 2.2500 94.777 0.65817
2-1/2 2.5000 105.113 0.72995
2-3/4 2.7500 115.449 0.80173
3 3.0000 126.301 0.87709 +.150″ -.010″ +.160″ -.010″
3-1/2 3.5000 146.972 1.02064
4 4.0000 168.264 1.16850 +.180″ -.010″ +.200″ -.010

 

Nickel 600 coil tykkelse diagram

Tykkelse (mm) 1000 Mindre enn eller lik Bredde < 1250 (mm) 630 Mindre enn eller lik bredde < 1000 (mm) 1250 Mindre enn eller lik Bredde < 1550 (mm)
0,40 Mindre enn eller lik T < 0,60 ±0.035 ±0.035 -
1,25 Mindre enn eller lik T < 1,60 ±0.060 ±0.055 ±0.060
1,60 Mindre enn eller lik T < 2,00 ±0.070 ±0.065 ±0.080
0,25 Mindre enn eller lik T < 0,40 ±0.035 ±0.030 -
0,80 Mindre enn eller lik T < 1,00 ±0.050 ±0.040 ±0.050
0,60 Mindre enn eller lik T < 0,80 ±0.040 ±0.040 -
1,00 Mindre enn eller lik T < 1,25 ±0.055 ±0.050 ±0.060

 

modular-1

ss@gneesteel.com

Se Inconel 600 stålplatedimensjoner (mm), standard platestørrelser og spolestørrelser, spolestørrelsestabell og Gnee Steel-platedimensjoner i rustfritt stål.

Sende bookingforespørsel

whatsapp

Telefon

E-post

Forespørsel