Feb 04, 2026 Legg igjen en beskjed

Inconel 601 rørfittings størrelsesinformasjonstabell

Inconel 601 rørdeler dimensjoner

ASME b16.9 Beslag
Normal rørstørrelse
ANSI b16 9 rørkobling O
D Y
Vegg Tykkelse T
(Røralbue Sch.)
LR 45 grader albuerSentrum til AnsiktB SR 45 Deg Albuer
Vekt
LR 90 Deg AlbuerSentrum til AnsiktA LR 90 Deg Albuer Vekt under SR 90 Deg AlbuerSentrum til AnsiktA SR 90 Deg Albuer Vekt under
millimeter tomme. millimeter millimeter Rute millimeter kilogram millimeter kilogram millimeter kilogram
15 1/2" 21.3 2.78 STD 15.9 0.04 38.1 0.08 – –
      3.73 X.S 15.9 0.05 38.1 0.10 – –
20 3/4" 26.7 2.87 STD 11.1 0.04 28.6 0.08 – –
      3.91 X.S 11.1 0.05 28.6 0.11 – –
25 1" 33.4 3.38 STD 22.2 0.09 38.1 0.15 25.4 0.11
      4.55 X.S 22.2 0.11 38.1 0.19 25.4 0.14
32 11/4" 42.2 3.56 STD 25.4 0.14 47.6 0.28 31.75 0.18
      4.85 X.S 25.4 0.2 47.6 0.39 31.75 0.24
40 11/2" 48.3 3.68 STD 28.6 0.2 57.1 0.4 38.1 0.26
      5.08 X.S 28.6 0.25 57.1 0.5 38.1 0.35
50 2" 60.3 3.91 STD 34.9 0.36 76.2 0.72 50.8 0.5
      5.54 X.S 34.9 0.5 76.2 1.0 50.8 0.68
65 21/2" 73.0 5.16 STD 44.4 0.73 95.2 1.46 63.5 0.95
      7.01 X.S 44.4 0.91 95.2 1.82 63.5 1.27
80 3" 88.9 5.49 STD 50.8 1.1 114.3 2.18 76.2 1.45
      7.62 X.S 50.8 1.45 114.3 2.86 76.2 1.95
100 4" 114.3 6.02 STD 63.5 2.1 152.4 4.2 101.6 2.8
      8.56 X.S 63.5 2.9 152.4 5.7 101.6 3.9
125 5" 141.3 6.65 STD 79.4 3.4 190.0 6.8 127.0 4.8
      9.5 X.S 79.4 5.0 190.0 10.0 127.0 6.5
150 6" 168.3 7.11 STD 95.2 5.1 229.0 10.1 152.4 6.8
      10.97 X.S 95.2 7.7 229.0 15.3 152.4 10.2
200 8" 219.1 8.18 STD 127.0 10.2 305.0 20.4 203.0 13.6
      12.7 X.S 127.0 15.5 305.0 30.9 203.0 20.9
250 10" 273.9 9.27 STD 159.0 18.1 381.0 36.1 254.0 24.1
      12.7 X.S 159.0 24.4 381.0 48.8 254.0 32.5
300 12" 323.9 9.52 STD 190.0 26.6 457.0 53.1 305.0 35.4
      12.7 X.S 190.0 35.0 457.0 70.0 305.0 46.7
350 14" 355.6 9.52 STD 222.0 34.1 533.0 68.1 356.0 45.4
      12.7 X.S 222.0 45.0 533.0 90.0 356.0 60.0
400 16" 406.4 9.52 STD 254.0 45.0 610.0 89.3 406.0 59.5
      12.7 X.S 254.0 59.0 610.0 118.0 406.0 78.7
450 18" 457.0 9.52 STD 286.0 56.5 686.0 113.0 457.0 75.6
      12.7 X.S 286.0 75.0 686.0 150.0 457.0 100.0
500 20" 508.0 9.52 STD 318.0 85.0 762.0 140.0 508.0 93.5
      12.7 X.S 318.0 112.5 762.0 186.0 508.0 124.0
600 24" 610.00 9.52 STD 381.0 101.5 914.0 203.0 610.0 135.0
      12.7 X.S 381.0 134.5 914.0 269.0 610.0 179.0

Sende bookingforespørsel

whatsapp

Telefon

E-post

Forespørsel