Oct 20, 2025 Legg igjen en beskjed

Monel 400 Cold Finished Seamless Pipe

 

Monel 400 Cold Finished Seamless Pipe

 

Monel 400 cold-finished seamless pipe is made from a nickel-copper alloy known for its high strength, toughness, and excellent corrosion resistance in seawater, acidic, and alkaline environments. The terms "cold-finished" and "seamless" indicate its precise dimensions, smooth surface finish, and increased strength achieved through cold working. It is widely used in the marine, chemical, and oil and gas industries, withstanding a wide range of temperatures from cryogenic to high.

Monel 400 Cold Finished Seamless Pipe
Monel 400 pipe

What are the specifications for Monel 400 pipe?

 

This grade of nickel-copper alloy is available in ASTM B165 and B725 specifications. Pipe is available in seamless, welded, electric-resistance-welded, and fabricated forms. ASME SB165 Monel 400 seamless pipe conforms to ASTM, ASME, and API standards and is available in nominal inside diameters ranging from 15 inches to 150 inches.

UNS N04400 Pipe Specification

ASTM B 165 ASME SB 165 / ASTM B 725 ASME SB 725, UNS 4400 Pipe
ASTM B165 monel 400 Seamless Pipe Size 4 to 219mm W. T.: 0.5 to 20mm
UNS N04400 Welded Pipe Size 5.0 - 1219.2 mm
Monel WERKSTOFF NR. 2.4360 EFW Pipe size 5.0 - 1219.2 mm
12 Swg., 10 Swg., 16 Swg., 14 Swg., 20 Swg., 18 Swg.,
400 Monel Pipe Schedule XS, SCH30, SCH40, XXS, SCH80, SCH120, SCH60, SCH140, STD, SCH10, SCH10S, SCH40S, SCH80, SCH20, SCH5, SCH160
monel 400 pipe Length
Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF, NO.1, NO.4, 2B, BA, HL, 8K, Mirror finish, etc
monel 400 are available in form of Round, Square, Hollow, Rectangular, Hydraulic, Coiled, Straight Pipes, "U" Shape, Pan Cake Coils etc.
Type of 400 Alloy Pipe Seamless / ERW/ EFW / Welded / Fabricated / CDW / DOM / CEW monel 400
monel 400 pipe End

 

Monel 400 pipe Chemical Composition Chart

C S
Monel 400 0.30 max 2.00 max 0.50 max 0.24max 28.0-34.0 2.50 max 63.00 min

 

ASME SB 165 Seamless Monel 400 Pipe Mechanical Behaviour

Yield Strength (0.2%Offset)
Monel 400 8.8 g/cm3 1350 ℃ (2460 ℃F) Psi – 80,000 , MPa – 550 Psi – 35,000 , MPa – 240 40 %

 

Wall Thickness of UNS N04400 Pipe

1/8" - 8" Upto 6 Meters SCH 5 to SCH 160
monel 400 Welded Pipe (in Stock + Custom Sizes) 5 mm - 1219.2mm 1 - 15 mm
monel 400 Seamless Pipe (Custom Sizes) 5 mm - 203.2mm

 

Monel 400 Cold Finished Seamless Pipe Applications
Marine: Fittings, fixtures, and components suitable for use in marine environments.
Chemical Processing: Equipment used to handle acids and other corrosive chemicals.
Oil & Gas: Processing equipment and components for the oil and gas industry.
General Purpose: Used in valves, pumps, propeller shafts, and various other high-strength, corrosion-resistant components.

Gnee Steel

 

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.