Apr 23, 2024 Legg igjen en beskjed

Hva brukes INCONEL til?

Hva brukes INCONEL til?

 

Inconel kjemisk sammensetning

KARAKTER ELEMENT (% ETTER MASSE)
NI CR FE MO NB CO MN CU AL TI SI C S P B
600 72.0 14.0–17.0 6.0–10.0       1.0 0.5     0.5 0.15 0.015    
617 44.2–56.0 20.0–24.0 3.0 8.0–10.0   10.0–15.0 0.5 0.5 0.8–1.5 0.6 0.5 0.15 0.015 0.015 0.006
625 58.0 20.0–23.0 5.0 8.0–10.0 3.15–4.15 1.0 0.5   0.4 0.4 0.5 0.1 0.015 0.015  
690 59.5 30 9.2       0.35 0.01 0.02   0.35 0.019 0.003    
718 50.0–55.0 17.0–21.0 balansere 2.8–3.3 4.75–5.5 1.0 0.35 0.2–0.8 0.65–1.15 0.3 0.35 0.08 0.015 0.015 0.006
X-750 70.0 14.0–17.0 5.0–9.0   0.7–1.2 1.0 1.0 0.5 0.4–1.0 2.25–2.75 0.5 0.08 0.01    

 

Inconel Ekvivalent materiale

STANDARD WERKSTOFF NR. UNS GOST AFNOR JIS BS EN ELLER
Inconel 600 2.4816 N06600 МНЖМц 28-2,5-1,5 NC15FE11M NCF 600 NA 13 NiCr15Fe ЭИ868
Inconel 601 2.4851 N06601 XH60BT NC23FeA NCF 601 NA 49 NiCr23Fe ЭИ868
Inconel 617 2.4663 N06617            
Inconel 625 2.4856 N06625 ХН75МБТЮ NC22DNB4M NCF 625 NA 21 NiCr22Mo9Nb ЭИ602
Inconel 690 2.4642 N06690            
Inconel 718 2.4668 N07718            
Inconel 725 - N07725            
Inconel X-750 2.4669 N07750            

 

Inconel og Monel
Inconel og Monel er begge nikkelholdige legeringer. Men i tillegg til å inneholde nikkel som deres primære legeringsmiddel, inneholder de også andre elementer som deres sekundære legeringsmidler. Monel, for eksempel, er sammensatt av kobber, som utgjør 30 til 40 prosent av dens totale vekt. Inconel inneholder krom som hjelpelegeringsmiddel. Når det gjelder egenskapene, er Monel en legering med middels ytelse, mens Inconel er en type med høy ytelse. Flere Inconel-legeringer er også kjent som superlegeringer fordi de har utmerket korrosjonsmotstand og utkonkurrerer flere konvensjonelle legeringer ved høye temperaturer. Monel er et binært metall i solid løsning, mens Inconel er en austenittisk høytemperaturlegering.

What is INCONEL used forWhat is INCONEL used forWhat is INCONEL used for

Inconel mekaniske egenskaper

  TETTHET SMELTEPUNKT STREKKSTYRKE AVKASTINGSSTYRKE (0,2 %OFFSET) FORLENGELSE
600 8,47 g/cm3 1413 grader (2580 grader F) Psi – 95,000 , MPa – 655 Psi – 45,000 , MPa – 310 40 %
601 8,1 g/cm3 1411 grader (2571 grader F) Psi – 80,000 , MPa – 550 Psi – 30,000 , MPa – 205 30 %
617 8,3 g/cm³ 1363 grader Større enn eller lik 485 MPa Større enn eller lik 275 MPa 25 %
625 8,4 g/cm3 1350 grader (2460 grader F) Psi – 135,000 , MPa – 930 Psi – 75,000 , MPa – 517 42.5 %
690 8,3 g/cm³ 1363 grader Større enn eller lik 485 MPa Større enn eller lik 275 MPa 25 %
718 8,2 g/cm3 1350 grader (2460 grader F) Psi – 135,000 , MPa – 930 Psi – 70,000 , MPa – 482 45 %
725 8,31 g/cm3 1271 grader -1343 grader 1137 MPa 827 MPa 20 %
X-750 8,28 g/cm3 1430 grader 1267 MPa 868 MPa 25 %

 

Monel-materialekvivalent

STANDARD WERKSTOFF NR. UNS GOST AFNOR JIS BS EN
Monel 400 2.4360 N04400 МНЖМц 28-2,5-1,5 NU-30M NW 4400 NA 13 NiCu30Fe
Monel 404 2.4867 N04404          
Monel 405   N04404          
Monel K500 2.4375 N05500          

Monel kjemisk sammensetning

HANDELSNAVN ASTM/AISI

LEGERINGSTYPE

UNS %CU %AL %TI %FE %MN %SI %NI
Monel 400 B 127, B 164 N04400 28-34     2,5 maks 2.0 maks 0.5 maks 63 min
Monel 401   N04401 28-34     2,5 maks 2.0 maks   63 min
Monel 404   N04404 Rem 0.05 maks   0.5 maks 0.1 maks 0.1 maks 52-57
Monel K-500 B 865 N05500 27-33 2.3-3.15 0.35-0.85 2.0 maks 1,5 maks 0.5 maks 63 min
Monel 405 B 164 N04405 28-34     2,5 maks 2.0 maks 0.5 maks 63 min

Monel mekaniske egenskaper

  TETTHET SMELTEPUNKT STREKKSTYRKE AVKASTINGSSTYRKE (0,2 %OFFSET) FORLENGELSE
Monel 400 8,8 g/cm3 1350 grader (2460 grader F) Psi – 80 000, MPa – 550 Psi – 35000, MPa – 240 40 %
Monel 404 8,91 g/cm3 1300 - 1350 grad 70 KSI min (483 MPA min) 25 KSI min (172 MPA min) 35 %
Monel 405 8,80 g/cm3 1300 - 1350 grad 550 Mpa 240 Mpa 40 %
Monel K500 8,44 g/cm3 1350 grader (2460 grader F) Psi – 160 000, MPa – 1100 Psi – 115 000 , MPa – 790 20 %