SS310 Stainless Steel Buttweld Pipe Fittings
video

SS310 Stainless Steel Buttweld Pipe Fittings

SS 310 Buttweld fittings are superbly resistive to corrosion in various affecting mediators. These are defended against pitting and provide anti-rust surfaces. Our fitting are finely surfaced inside to allow even flow through it that reduces corrosion and oxidation. Also, our fittings provide resistance to pressure turbulence due to their excellent strength. SS 310S Buttweld fittings are less tending to embrittlement as well as sensitization.
Sende bookingforespørsel
Chat nå

Som en ledende leverandør og produsent i Kina, leverer GNEE Steel kostnads-effektive nikkel-baserte legeringsprodukter.

produkt introduksjon

 

SS 310 Buttweld fittings are superbly resistive to corrosion in various affecting mediators. These are defended against pitting and provide anti-rust surfaces. Our fitting are finely surfaced inside to allow even flow through it that reduces corrosion and oxidation. Also, our fittings provide resistance to pressure turbulence due to their excellent strength. SS 310S Buttweld fittings are less tending to embrittlement as well as sensitization.

0917 32

SS 310 is specifically designed for high-temperature corrosion-resistant applications. It is austenitic and composed of high-value chromium and reasonable nickel value. Carbon value is lessened to 0.08, forms SS 310S grade, that is used because of the easiness of production. It prevents from sulfidation and carburizing atmospheres. It can be easily welded and is more corrosion resistant than most heat-resistant alloys.

SS 310 1.4841 S31000 SUS 310 310S24 20Ch25N20S2 X15CrNi25-20
SS 310S 1.4845 S31008 SUS 310S 310S16 20Ch23N18 X8CrNi25-21
C P S
SS 310 0.015 max 2.0 0.15 0.020 max 0.015 max 24.00 – 26.00 0.10 19.00 – 21.00 54.7 min
SS 310S 0.08 max 2.0 1.00 0.045 max 0.030 max 24.00 – 26.00 0.75 19.00 – 21.00 53.095 min

4 06