2.4665 Wrought Nickel Chromium Molybdenum Alloy Strip
video

2.4665 Wrought Nickel Chromium Molybdenum Alloy Strip

We are a reputable manufacturer specializing in the production of DIN 17744 Wrought Nickel Chromium Molybdenum Alloys. With a focus on professionalism and high technical expertise, we employ state-of-the-art VIM and VAR equipment to ensure top-quality products. Our commitment to efficiency is reflected in our swift delivery times, and we accommodate small order quantities to meet your specific needs. We invite you to inquire about our products and services. Your satisfaction is our priority.
Sende bookingforespørsel
Chat nå

Som en ledende leverandør og produsent i Kina, leverer GNEE Steel kostnads-effektive nikkel-baserte legeringsprodukter.

produkt introduksjon

 

2.4665 alloy is a kind of nickel-based superalloy with high iron content, which is mainly strengthened with chromium and molybdenum solid solution. It has good nutrient resistance and corrosion resistance, medium lasting and creep strength below 900 degree , and good cold and hot processing formability and weldability. Used in the manufacture of combustion chamber components and other high-temperature components of aircraft engines, long-term use below 900 degree C, short-term operating temperature up to 1080 degree C. The main products supplied are sheet, strip, pipe, bar, forgings, ring and precision

t01cd4d7cc4bedc2cdf




0.1 0.12 0.15 0.2mm thick 8mm wide nickel strip

1.make the battery pack more powerful, save energy.
2. it's easy welding, stable connection.
3. Good tension and easy operate assembly.
4. High Electrical Conductivity.

1.Spot welding is good.
2.The resistance is lower.
3. Battery discharge time longer.
4. The battery spot welding is stronger.

this product is mainly used in manufacturing nickel-cadmium battery, nickel-hydrogen battery, lithium cell, assembled battery, as well as industries of electric tool and special lights.

20231027152515

 

Q1:What product information must I provide before making a purchase?

Q2:What shipping ports are there?

Q3:What are your payment terms?
30% T/T in advance and 70% balance before shipment or based onBL copy or LC at sight.

Populære tags: 2.4665 wrought nickel chromium molybdenum alloy strip, China 2.4665 wrought nickel chromium molybdenum alloy strip suppliers

Sende bookingforespørsel

whatsapp

Telefon

E-post

Forespørsel